Dầu tôi nhiệt luyện VBC BW-1280C Dầu tôi nhiệt luyện VBC BW-1280C

VBC BW-1280C is high quality quenchant formulated from premium hydrocracked base oil stock. BW-1280C is designed for operating conditions that require accelerated oil to develop maximum hardness with minimum distortion and shiny surface.

Dầu tôi nhiệt luyện VBC BW-1280C Sản phẩm khác Số lượng: 1 sản phẩm
Dầu tôi nhiệt luyện VBC BW-1280C
  •  
Dầu tôi nhiệt luyện VBC BW-1280C
  • Đăng ngày 23-11-2016 12:24:02 AM - 1473 Lượt xem
  • Giá bán: Liên hệ
  • VBC BW-1280C is high quality quenchant formulated from premium hydrocracked base oil stock. BW-1280C is designed for operating conditions that require accelerated oil to develop maximum hardness with minimum distortion and shiny surface.


Dầu tôi nhiệt luyện VBC BW-1280C

Description ( Mô tả)
VBC BW-1280C is high quality quenchant formulated from premium hydrocracked base oil stock. BW-1280C is designed for operating conditions that require accelerated oil to develop maximum hardness with minimum distortion and shiny surface.

Benefits ( Lợi ích tính năng)

- Excellent thermal stability – Recommended for use when part must retain a bright finsh.
- Controlled cooling rate – Provide a high initial cooling rate including maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stress and metal distortion.
- Exceptional oxidation resistance – Results in extended oil life, brighter quenched part, and greater cooling efficiency of oil.
- Stable additive package – Minimal loss of additives due to extended use

Application (Ứng dụng)

At open type quench tank, BW-1280C is recommended for use
– In hardening, carburizing and carbonitriding of forged or pressed steel
– In hardening of small or thick bearing steel.
– In hardening of carbon tool steel and alloy steel. Application
– In carburizing and carbonitriding of low-alloy st

Package ( Bao bì)

200L/ Phuy

Sản phẩm bạn vừa xem
Thống kê truy cập
  • Đang truy cập41
  • Hôm nay4,288
  • Tháng hiện tại10,245
  • Tổng lượt truy cập10,713,880

Copyright © 2016 Công ty TNHH TM&DV Kỹ thuật Hạnh San | design by: dangkha - 0974 624 069

Bạn đã không sử dụng Site, Bấm vào đây để duy trì trạng thái đăng nhập. Thời gian chờ: 60 giây